kersploosh@sh.itjust.worksM to Engineering@sh.itjust.works · 8 days agoOil quenchingi.imgur.comvideomessage-square17linkfedilinkarrow-up1217arrow-down13file-text
arrow-up1214arrow-down1videoOil quenchingi.imgur.comkersploosh@sh.itjust.worksM to Engineering@sh.itjust.works · 8 days agomessage-square17linkfedilinkfile-text
Watching heavy machinery never gets old. Source: https://imgur.com/gallery/oil-quenching-y3oiCKG#/t/toolgifs
minus-squareTar_Alcaran@sh.itjust.workslinkfedilinkarrow-up4·8 days agoIt should be. If you heat it all the way through, you get more heat-stress. Ideally, you only want the outside hot (and then cold again) to surface-harden it. You don’t need the middle bits hardened, after all.
It should be. If you heat it all the way through, you get more heat-stress. Ideally, you only want the outside hot (and then cold again) to surface-harden it. You don’t need the middle bits hardened, after all.